Microstructural analysis of a Mg-Zn alloy deformed at room temperature by high-pressure torsion (HPT) indicates that fine-scale precipitation occurs even without post-deformation heat treatment. Small-angle X-ray scattering detects precipitates with radii between 2.5-20 nm after one rotation, with little increase in particle size or volume fraction after 20 rotations. High resolution electron micrographs identify grain boundary precipitates of monoclinic MgZn phase after three rotations and MgZn after 20 rotations.